Abstract
The thermal diffusivity has been measured for the Polypyrrole-Polyethylene Glycol (PPy-PEG) composite films by the open photoacoustic method. The experimental data were analyzed for thermal diffusivity by fitting procedure. The different process parameters such as different concentrations of insulating polymer, monomer and electrolyte and the different voltages used to prepare the PPy-PEG composite films brought changes in thermal diffusivity. The process condition of 0.20 M pyrrole, 0.10 M p-toluene sulfonate and 1×10-3 M PEG at 1.20 volt (vs SCE) appeared as the optimum condition and the PPy-PEG composite film produced from this optimum condition shows the highest thermal diffusivity (7.88×10-7 m2 s-1).
Licence and reuse
Free to read. This article carries the publisher’s copyright, as printed on it: © 2009 Science Publications. It is free to read; ask us before reusing it.
How to reuse this articleResponses (0)
About this article
Lim, M. Y., Yunus, W. M. M., Kassim, A. & Mahmud, H. (2009). Photoacoustic Measurement of Thermal Diffusivity of Polypyrrole Conducting Polymer Composite Films . American Journal of Applied Sciences, 6(2), 313–316. https://doi.org/10.3844/ajassp.2009.313.316
- Licence
- © Science Publications
- Issue
- Volume 6, Issue 2
- Policies
- Editorial independenceUse of generative AIData availabilityAppeals and complaints
- Version
- Version of record